Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Smart Card" in Material Data Center leads to the following information:

Tradename: Smart Card
Family: EP
Producer: Isola GmbH
3 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2005-11-21, Production Cell Offers Complete Solution
... 621 CNC stacking robot, which has already been used hundreds of times in the past, in combination with the W 627 HSS insert and removal unit (manufacturer: Wittmann Robot Systems GmbH, Schwaig), which has been used successfully in the smart card technology for nearly ten years, together form an effective automatic production cell when used with part-specific grippers and stacking magazines. The production cell ideally combines all the following operations in a very small working area: - remove ...

Kunststoffe international, 2011-06-20, Interaction with the User
... an example of innovative printed electronics with high innovation potential. Such smart labels will in future be used in very diverse areas, such as marketing, brand protection and games with high customer benefit. Printed smart card as gift voucher (figures: PolyIC) Fig. 1. Printed interactive optical labels (smart labels) from the roll Fig. 2. A radio-activated display consists of a thin flexible display (centre top and top right) with receiver circuit (right) and an activation unit (left) Fi...

Kunststoffe international, 2012-06-25, Taking Control
...w behavior of the melt, let alone the shrinkage of the part itself. This requires additional information from a temperature sensor which has to be located at a defined distance from the pressure sensor [2]. During the production of a two component smart card seal (Title photo) by Continental Automotive GmbH at their Villingen-Schwenningen facility in Germany a cavity pressure transducer and tool wall temperature sensor determine the flow properties, compression and shrinkage of the hard componen...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.